Showing 3 results for Nickel-Based Superalloy
Sajad Ghaemifar, Hamed Mirzadeh,
Volume 20, Issue 4 (12-2023)
Abstract
Phase transformations and the evolution of hardness during elevated-temperature annealing of Inconel 718 superalloy manufactured by the laser powder bed fusion (L-PBF) were investigated. The microstructural evolution, elemental analysis, phase formation, and hardening were characterized by scanning electron microscopy, energy-dispersive spectroscopy, X-ray diffraction, and Vickers indentation test, respectively. It was observed that the effect of annealing treatments is directly governed by the annealing parameters (i.e. time and temperature), for which the hardness measurement as a fruitful and convenient tool can reveal this effect. The increase of the hardness, which was obtained by the annealing (aging) treatments at the temperature range of 800-900 °C, indicated precipitation of the Ni3Nb γ˝ strengthening phase; while owing to the coarsening of precipitates as a results of overaging at this temperature range, the hardness decreased. For instance the length and aspect ratio of precipitates in the aged sample at 800 °C for 1 h is 67.14 nm and 0.32, respectively; while these values in the aged sample at 800 °C for 8 h is 78.34 nm and 0.44, respectively. On the other hand, the decrease of the hardness at temperatures of 950 and 1000 °C was attributed to the decrease of dislocation density in conjunction with the Ni2Nb Laves phase dissolution. Hence, it is crucial to determine the annealing parameters according to the required microstructure and properties.
Seyed Hossein Razavi, Amirhossein Riazi, Alireza Khavandi, Mostafa Amirjan, Mohsen Ostad Shabani, Hossein Davarzani, Yazdan Shajari,
Volume 22, Issue 2 (6-2025)
Abstract
Additive manufacturing (AM) of metallic parts has gained significant attention in recent years due to its ability to produce components without traditional tooling such as molds, melting furnaces, or extensive raw material preparation. Its unique capability to fabricate complex geometries has revolutionized part design and enabled substantial weight reduction. This review first outlines the development trajectory of metal-based AM, with a particular focus on laser-based fusion methods, including Laser Powder Bed Fusion (LPBF) and Direct Laser Deposition (DLD). Understanding this evolution helps researchers identify both the capabilities and limitations of AM technologies, thereby enhancing their application in areas such as prototyping, mass production, and repair. Each metal possesses unique physical and chemical properties, which often make traditional manufacturing methods more challenging—especially for alloys with high strength, hardness, or temperature resistance. In this context, the review then focuses on nickel-based superalloys (NBSAs), which are widely used in high-temperature and high-stress environments but are particularly difficult to process using conventional techniques. Their application serves as a representative case study for evaluating the performance and feasibility of AM techniques for advanced materials. Furthermore, the future prospects of AM are discussed, including advancements in monitoring systems, integration of machine learning, and the development of AM-specific alloys. As a novel aspect, this work compares LPBF and DLD in terms of their advantages, limitations, and resulting material properties, along with a comparison to traditional manufacturing methods such as casting and wrought processing.
Hamed Heydari, Mojtaba Zolfaghari,
Volume 23, Issue 3 (9-2026)
Abstract
Twin-boundary engineering provides an effective approach for tailoring the mechanical response of nickel-based superalloys; however, the density-dependent atomistic mechanisms remain insufficiently understood in explicit dual-phase γ/γ′ microstructures. Molecular dynamics simulations were performed on a single-crystal model and models containing one, two, and eight twin boundaries oriented perpendicular to the loading direction. The tensile response was analyzed in conjunction with dislocation-density evolution, microstructural changes, and Constructed-surface-mesh analysis to characterize crack initiation and growth. The TB1 model exhibited higher yield stress and strain than the single-crystal model because the isolated twin boundary impeded dislocation motion. In contrast, TB2 and TB8 yielded at lower stresses and strains because the increased twin-boundary density introduced additional preferential nucleation sites at the twin boundaries and twin-boundary/γ–γ′ interface intersections. Despite its earlier yielding, TB2 exhibited the highest ultimate stress among all models and the highest ultimate strain among the twinned models. This behavior was attributed to deformation partitioning between two comparatively stable twin boundaries, which promoted distributed precipitate shearing, dislocation storage, and sustained strain hardening. TB8 exhibited the highest initial dislocation density, followed by a decrease during plastic deformation associated with twin-boundary migration, defect rearrangement, and strain localization. Constructed-surface-mesh analysis further showed that crack initiation was delayed to a strain of approximately 0.07356 in TB2, compared with approximately 0.066 in TB1 and TB8. Crack propagation occurred predominantly along the twin boundaries and γ/γ′ phase interfaces. These findings reveal a non-monotonic, density-dependent transition from barrier-controlled strengthening in TB1 to deformation-partitioning-assisted hardening in TB2 and boundary-migration-assisted, localization-dominated softening in TB8.